Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitable for automotive, engineering, electrical and consumer goods industry. With the increasing content of GF also the toughness, tensile and bending strength, modulus in tension and bending increase and the shrinkage decreases as well as the heat application increases up to 130°C. Additional drying of the material is not necessary. Delivered in natural and in the full RAL color scale. Production of the fuel tank caps for the transport vehicles, shells for the textile industry.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0132 cm/cm
0.0132 in/in
STN 64 0808
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
STN EN ISO 527-2
Elongation at Break 4.0 %
4.0 %
STN EN ISO 527-2
Tensile Modulus 4.90 GPa
711 ksi
STN EN ISO 527-2
Flexural Strength 85.0 MPa
12300 psi
STN EN ISO 178
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Charpy Impact Unnotched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
STN EN ISO 75/A
Vicat Softening Point 130 °C
266 °F
B; STN EN ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi