Material Notes:
Information provided by HexCel
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Resin Density
2.60 g/cc
0.0939 lb/in³
Fibre Density
Mechanical Properties Metric English Comments
Tensile Strength, Yield 280 MPa
40600 psi
90º, RT, Dry; EN2561
Tensile Modulus 17.0 GPa
2470 ksi
90º, RT, Dry; EN2561
Shear Strength 49.7 MPa
7210 psi
90º, ILSS Short Beam, RT, Dry; EN2563
55.0 MPa
7980 psi
0º, ILSS Short Beam, RT, Dry; EN2563
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 - 130 °C
248 - 266 °F
Epoxy Matrix Limit
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.015
Fiber Volume (%) 35