Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Optrene 10GF Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ovation Polymers
Trade Name Optrene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Optrene 10GF Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemically coupled glass reinforced(10%) polypropylene with high strength and HDT.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 0.995 g/cc
0.995 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0024 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0024 - 0.0030 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm

@Thickness 3.17 mm
0.010 - 0.014 in/in

@Thickness 0.125 in
Melt Flow 13.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
50 mm/min; ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 55.0 MPa
7980 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C

@Thickness 3.20 mm
293 °F

@Thickness 0.126 in
unannealed; ASTM D648