Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.70 GPa | 247 ksi | ASTM D638 |
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | |
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO.527 DIN.53455 |
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ASTM D638 |
NCMT NanoPAC™ N10 High Performance Polypropylene Nanocomposite Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Electrical Appliances Toys IndustryI.. |
|||
Tensile Modulus | 1.70 - 2.50 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
247 - 363 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
DSM Akulon® F223-DH (Cond.) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9523 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9523 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9523 is dev.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
Lanxess Pocan® S 1506 000000 PBT PBT, non-reinforced, injection molding extrusion, impact modified |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
Lanxess Pocan® S 1506 901510 PBT PBT, injection molding grade, non-reinforced, elastomer-modified, high impact strength, even at low temperatures |
|||
Tensile Modulus | 1.70 - 2.50 GPa @Thickness 2.00 mm |
247 - 363 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000 is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-2 |
Total PPH 9020 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9020 is a clarified homopolymer.ApplicationATOFINA Polypropylene PPH 9020 has been designed with a very high stiffness and an outstanding transparency. It is particularly .. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Tensile Modulus | 1.70 GPa @Temperature -70.0 °C |
246 ksi @Temperature -94.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ISO 527-1/-2 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | ASTM-D790 |
Polyram RamOfin PPC370B73 Polypropylene, 73% Mineral Filled 73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.70 GPa | 247 ksi | 1 mm/min |
Arkema Group Oroglas® SG 10 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no advers.. |