Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.995 g/cc | 0.995 g/cc | ASTM D792 |
Ovation Polymers Optrene 10GF Polypropylene Chemically coupled glass reinforced(10%) polypropylene with high strength and HDT.Information provided by Ovation Polymers |
|||
Specific Gravity | 0.995 g/cc | 0.995 g/cc | ASTM D792 |
Ovation Polymers OPTRENE 10GF Polypropylene, 10% Glass Reinforced Properties of chemically coupled glass reinforced (10 %) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Specific Gravity | 0.995 g/cc | 0.995 g/cc | |
Dow Corning 24 EMULSION Dow Corning® 24 Emulsion is a stable, water-dilutable emulsion suitable for the food processing industry. It produces a slippery film upon water evaporation of the product.Information provided by D.. |
|||
Specific Gravity | 0.995 g/cc | 0.995 g/cc | |
Chesterton 989 Release Compound Description: Chesterton® 989 Release Compound is a highly effective, release agent containing no CFC's or organic solvents. Environmental responsibility and concern for worker safety need not mean .. |