Material Notes:
Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms.
Physical Properties Metric English Comments
Density 7.90 g/cc
0.285 lb/in³
RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 585 MPa
84800 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 275 MPa

@Strain 0.200 %
39900 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Elongation at Break 35 %
35 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 200 GPa
29000 ksi
RT
172 GPa

@Temperature 400 °C
24900 ksi

@Temperature 752 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 100 °C
8.89 µin/in-°F

@Temperature 212 °F
17.5 µm/m-°C

@Temperature 400 °C
9.72 µin/in-°F

@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C
0.120 BTU/lb-°F
RT
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
RT
20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 17.3 %
17.3 %
Iron, Fe 74.45 %
74.45 %
Nickel, Ni 8.2 %
8.2 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Users viewing this material also viewed the following: