Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 20.0 - 100 °C |
0.0000730 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 20.0 - 100 °C |
0.0000730 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior .. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 20.0 - 100 °C |
0.0000730 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 20.0 - 100 °C |
0.0000730 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | |
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 23.0 °C |
0.0000730 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 347 Chromium-Nickel Steel Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 23.0 °C |
0.0000730 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Electrical Resistivity | 0.0000730 ohm-cm @Temperature 20.0 - 100 °C |
0.0000730 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |