Electrical Properties Metric English Comments
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4305 Austenitic Stainless Steel
Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms.
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms.
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 20.0 - 100 °C
0.0000730 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel
Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 20.0 - 100 °C
0.0000730 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel
Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior ..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 20.0 - 100 °C
0.0000730 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel
CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 20.0 - 100 °C
0.0000730 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel
CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 23.0 °C
0.0000730 ohm-cm

@Temperature 73.4 °F
Crucible Steel 347 Chromium-Nickel Steel
Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 23.0 °C
0.0000730 ohm-cm

@Temperature 73.4 °F
Crucible Steel 348 Chromium-Nickel Steel
Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..
Electrical Resistivity 0.0000730 ohm-cm

@Temperature 20.0 - 100 °C
0.0000730 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k..