Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This rigid polyurethane foam system is one of a family of polymer systems developed by Northstar Polymers for specific applications. Urethane foams molded with this system exhibit closed cell structure, and its high-density foam structure provides a very good lord bearing capability. The both components are low viscosity liquid and together with its easy mixing ratio of 1: 1 by volume, this material is ideal as a bonding agent structural composite. A user can mix and pour the mixture with common tools without an expensive casting/spray machine. This foam can also be mix/cast by a meter mixing machine. This foam do not use a volatile auxiliary blowing-agent and can be operated in a ambient workplace without being flame/spark-free environment. This combination of features makes MPL-R20B ideal for molded/cast structural parts, cat-in-place structural foam material, structural composites, and many other custom applications.Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Density 0.320 g/cc
0.0116 lb/in³
Free Rise Density
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
Flexural Strength 7.543 MPa
1094 psi
ASTM D-790
Compressive Strength 6.61 MPa

@Strain 10.0 %
959 psi

@Strain 10.0 %
ASTM D1621
Processing Properties Metric English Comments
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Mold Temperature 37.8 - 43.3 °C
100 - 110 °F
Cure Time 60.0 min

@Temperature 25.0 °C
1.00 hour

@Temperature 77.0 °F
De-mold Time
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 1.00 min
1.00 min
Descriptive Properties Value Comments
Appearance at 25°C Dark Yellow to Amber
Curing Agent PLA-012
Mixing Time 30
Prepolymer MNA-013
Weight Ratio 1:0.87
Prepolymer to Curing Agent Ratio