Solvay RHODAFAC® PA15 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAFAC® PA15 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYLATED ALCOHOL, PHOSPHATE ESTERCAS: 68439 – 39 - 4Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: EmulsifierInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
RPG18
Chemical Properties Metric English Comments
Total Acid Number 183 - 189
183 - 189
[mg KOH/g], #1; RPG44
320 - 330
320 - 330
[mg KOH/g], #2; RPG44
Processing Properties Metric English Comments
Moisture Content <= 4.0 %
<= 4.0 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Composition Active
0.96
Ionic Charge Anionic