Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 N-S20 Nylon 6.6 for injection molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 N-S20 Nylon 6.6 for injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, low viscosity, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 1.7 - 2.7 %
1.7 - 2.7 %
ISO 62
Water Absorption at Saturation 7.0 - 8.0 %
7.0 - 8.0 %
ISO 62
Viscosity Measurement 140
140
Viscosity index; ISO 307
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 102 MPa
14800 psi
ISO 2039-1
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527
Elongation at Break 29 %
29 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Strength 58.0 MPa
8410 psi
ISO 178
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB
NB
DIN 53453
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eA
1.80 J/cm²
8.57 ft-lb/in²
DIN 53453
1.30 J/cm²

@Temperature -40.0 °C
6.19 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V
600 V
CTI 100; IEC 112