Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2 in/min; ASTM D638 |
Network Polymers PC-1035 Description: Injection Molding Grade Low Gloss PolycarbonateInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 279 Water White Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 71.7 - 76.0 MPa | 10400 - 11000 psi | Average value: 74.4 MPa Grade Count:3 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Yield | 71.7 - 175 MPa | 10400 - 25400 psi | Average value: 121 MPa Grade Count:42 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M19 HS BK 19% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 19% Filler by Weight and Mineral Filler, 19% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Sumitomo Chemical Sumipex® MH Acrylic Resin, Heat Resistant Product CharacteristicsExtrusion GradeHeat ResistantInformation provided by Calsak Corporation |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP 60-8419G Clear Amorphous Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Entec Hyril® SAN500 Styrene Acrylonitrile Available in North America Features: Copolymer Form: PelletsInformation provided by Entec |