Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
Environmental Stress Crack Resistance 300 hour
300 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield 18.8 MPa
2730 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.620 GPa
89.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F
Users viewing this material also viewed the following: