Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 0.620 GPa | >= 89.9 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6432R (32604) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 0.620 GPa | >= 89.9 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6433R (32604) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
3M Dyneon™ PFA 6515N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ EP2015/60 medium melt flow, 690 MPa flexural modulus, extrusion coating grade, specialty polypropylene copolymer has a very good balance of properties and processability. Th.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 0.620 GPa @Strain <=0.250 % |
89.9 ksi @Strain <=0.250 % |
ISO 178 |
Total MDPE HF 513 Medium Density Polyethylene, Blown Film MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
Total PPR 7425 Polypropylene, Injection Molding Grade Random copolymer for injection moldingClarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.Impact - FINA 7425 produced molded parts with measurably impro.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | 2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationExcellent impac.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM Test |
BASF Ultramid® 8350 HS PA6 (Conditioned) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
Ashley Polymers Ashlene® D927 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
Ashley Polymers Ashlene® L927 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability, and low moisture absorption. Also availab.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM D790 |
3M Dyneon™ PFA 6515 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | |
3M Dyneon™ PFA 6515NZ Perfluoroalkoxy Fluorothermoplastic PFA designed for higher speed or higher shear processing such as injection molding and wire insulation. Demonstrates universal chemical and solvent resistance, high dielectric strength, excellent we.. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | ASTM Data |
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Flexural Modulus | 0.620 GPa | 89.9 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® D160HS TPO
(discontinued **) Description: DEXFLEX® D160HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require excellent durability, low-temperature impact resistance, low ther.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Flexural Modulus | 0.620 - 3.20 GPa | 89.9 - 464 ksi | Average value: 1.41 GPa Grade Count:154 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |