NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids, ice cream containers.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 36.0 cm
14.2 in
NOVA Snake Flow Test
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 0.760 GPa
110 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 113 °C
235 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F
Users viewing this material also viewed the following: