Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
NCMT Method
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D638
Elongation at Break <= 60 %
<= 60 %
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temp.; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved