Mytex Polymers AS23K-01 Polypropylene, Talc filled, Compounded, Non-UV stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS23K-01 Polypropylene, Talc filled, Compounded, Non-UV stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A non-UV stabilized talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.004 g/cc
0.03627 lb/in³
ASTM D792
Melt Flow 17 g/10 min
17 g/10 min
ASTM D1238
Ash 15 %
15 %
ISO 3451-1
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min; ISO 527
Flexural Modulus 2.132 GPa
309.2 ksi
Chord; 2 mm/min; 64 mm Span; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²

@Temperature -40.0 °C
0.952 ft-lb/in²

@Temperature -40.0 °F
ISO 180
4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179 / 1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75