Polymer Property : Density = 0.03627 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.004 g/cc
0.03627 lb/in³
ASTM D792
Mytex Polymers AS23K-01 Polypropylene, Talc filled, Compounded, Non-UV stabilized
Description: A non-UV stabilized talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation pro..