Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.004 g/cc | 0.03627 lb/in³ | ASTM D792 |
Mytex Polymers AS23K-01 Polypropylene, Talc filled, Compounded, Non-UV stabilized Description: A non-UV stabilized talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation pro.. |