Mytex Polymers AN18KW-01 FK Polypropylene, Rubber modified

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AN18KW-01 FK Polypropylene, Rubber modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rubber modified polypropylene produced for automotive interior applications using Mytex® Technology. Specifically designed to achieve ductile performance at cold temperatures during air bag deployment.Key Applications: Air bag deployable pillar and airbag trimInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ISO 1183
Melt Flow 17 g/10 min
17 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
50 mm/min; ISO 527
Flexural Modulus 0.700 GPa
102 ksi
Tangent; 1.3 mm/min; ISO 178
Izod Impact, Notched (ISO) 50.0 kJ/m²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C
145 °F
ASTM D648