Multibase Nylex™ 2185 Polyamide + PP

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Multibase
Trade Name Nylex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Nylex™ 2185 Polyamide + PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM 792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Strength 43.4 MPa
6300 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Gardner Impact 16.9 J
12.5 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Unannealed; ASTM D648
Vicat Softening Point 165 °C
329 °F
ASTM D1525