Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 5400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Multibase Nylex™ 2185 Polyamide + PP
Forms: PelletsInformation provided by Multibase
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced  (discontinued **)
Key Features: Electrostatic DissipativeRosite Conductive C used in applications such as molded paper guides in printers and plotters. Conductive C is the UL recognition.Information provided by Onei..
Tensile Strength, Ultimate 37.3 MPa
5400 psi
DIN 53455; ASTM D638
Kolon KOPEL® KP3363 General Purpose TPE Resin
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.
Tensile Strength, Ultimate 37.3 MPa
5400 psi
ASTM D412
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 37.3 MPa
5400 psi
ASTM D412
SK Chemicals SKYTHANE® S195A C series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 37.3 MPa
5400 psi
ASTM D412
SK Chemicals SKYTHANE® 470A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
Williams Advanced Alloys WS238 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Injection molding homopolymerNucleation - FINA 3620WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi- cavity molds.Antistat - FINA 3620WZ con..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D412/D638
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane
Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D412
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638
Buckeye Polymers BP ABS 6432 WS ABS
ABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing and outs..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
BCC Products BC 7009-2 Epoxy Casting
BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
AIM 47 Fusible Bismuth Alloy
Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D412
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod..
Tensile Strength, Ultimate 37.2 MPa
5400 psi
ASTM D638-95
Multibase Multi-ABS 3075 High Impact
Data provided by Multibase.
Copyright © lookpolymers.com All Rights Reserved