Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ASTM D955
Melt Flow 16.5 g/10 min
16.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 41.4 MPa
6000 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
73°F; ASTM D256
Gardner Impact 4.519 J
3.333 ft-lb
ASTM D3029