Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Multibase Multi-Pro® 4615 X White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Flexural Yield Strength | 41.4 - 81.4 MPa | 6000 - 11800 psi | Average value: 63.3 MPa Grade Count:108 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Global HI-830 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Flexural Yield Strength | 41.4 MPa @Temperature 23.0 °C |
6000 psi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene HI830 Polystyrene APPLICATIONS: EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES Statiblend® ABS FR AS BN Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES HiFill FR® PP GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 350E0096912 Natural, Trsp Cellulose Acetate Propionate Plasticizer 13%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 41.4 - 68.9 MPa | 6000 - 10000 psi | Average value: 58.6 MPa Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |