Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 2507 T NAT 25% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 2507 T NAT 25% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moisture is less than 0.06%. Multi-Pro 2507 T Natural is designed for high impact and high flexural strength. It can easily be colored and is FDA approved.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792-91
Melt Flow 6.5 g/10 min
6.5 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.30 MPa
334 psi
ASTM D638-95
Elongation at Break 50 %
50 %
ASTM D638-95
Flexural Strength 4.50 MPa
653 psi
ASTM D790-95
Flexural Modulus 2.069 GPa
300.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256-93a
Gardner Impact 9.30 J
6.86 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
ASTM D648-95
Copyright © lookpolymers.com All Rights Reserved