Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 9.30 J | 6.86 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 2507 T NAT 25% Filler Content Polypropylene Moisture is less than 0.06%. Multi-Pro 2507 T Natural is designed for high impact and high flexural strength. It can easily be colored and is FDA approved.Data provided by Multibase. |