Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2502 CU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648-95 |
Multibase Multi-Pro® 2507 T NAT 25% Filler Content Polypropylene Moisture is less than 0.06%. Multi-Pro 2507 T Natural is designed for high impact and high flexural strength. It can easily be colored and is FDA approved.Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 3.20 mm |
262 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 6.40 mm |
262 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 6.40 mm |
262 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 - 160 °C | 262 - 320 °F | Average value: 136 °C Grade Count:13 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 6.40 mm |
262 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 6.40 mm |
262 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 6.40 mm |
262 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 195 PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 3.20 mm |
262 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C @Thickness 3.20 mm |
262 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL NF1030 PPE+PS (Asia Pacific) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | Unannealed; ASTM D648 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Tipco Tipcolene® CR 7228 - 30% Talc/Mineral Reinforced Polypropylene Copolymer 30% Mineral Reinforced PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | |
Covestro Bayblend® T 84 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ISO 75-1,-2 |
Covestro Bayblend® T85 SG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ISO 75-1/-2 |
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® 1021 Polycarbonate A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® 1641 Polycarbonate A general purpose injection molding grade, natural resin, UL approved. Also available as: 1641R (with release); 1643 (with UV stabilizers); 1643R (with release and UV stabilizers).Data provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPP C 200-2 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® 1041BU Polycarbonate A general purpose injection molding grade, in black. Also available as: 1043BU (with UV stabilizers).Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® 1051 Polycarbonate A general purpose injection molding grade, natural resin. Also available as: 1051R (with release), 1053 (with UV stabilizers), 1053R (with release and UV stabilizers).Data provided by the manufactu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® 1621 Polycarbonate A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 °C | 262 °F | ASTM D648 |
Ashley Polymers Ashlene® P1021R Polycarbonate A prime general purpose injection molding grade, natural resin with easy mold release.Data provided by the manufacturer |