Zeon Chemicals Zealloy® 1422 Modifier for Thermoplastics

Category Polymer , Thermoset
Manufacturer Zeon Chemicals
Trade Name Zealloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zealloy® 1422 Modifier for Thermoplastics.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zealloy 1422 is a copolymer of butadiene and acrylonitrile of medium oil resistance. It is furnished as a finely-divided powder. Sufficient antioxidant is added during manufacture for normal storage conditions.Very fine cross linked powder used as a flexibilizer for PVC compounds.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Particle Mesh Size 40 Mesh
40 Mesh
90-100%; US std sieve
Ash 4.4 - 8.9 %
4.4 - 8.9 %
Zeon Test #1502
Thermal Properties Metric English Comments
Shrinkage 4.00 - 20.0 %

@Temperature 10.0 - 21.1 °C
4.00 - 20.0 %

@Temperature 50.0 - 70.0 °F
Mill Shrinkage; Zeon Test #820
Descriptive Properties Value Comments
Heat Loss (%) Max 0.6