Tensile Strength, Ultimate 10.5 MPa
1530 psi
ASTM D638
Multibase Multi-Flex® TEA 1004 TPO Thermoplastic Polyolefin Elastomer
Features: Adhesion, GoodPaintableWeather Resistance, Good Forms:PelletsUses: Automotive ApplicationsSealsToothbrush HandlesInformation provided by Multibase
Tensile Strength, Ultimate 10.5 MPa
1530 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 3075 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..