Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TSE 3221 is a one-component, flowable, heat curing adhesive which is translucent in color and offers primerless adhesion to a wide variety of substrates. This product requires an elevated temperature cure and exhibits very low linear shrinkage.Key Performance Properties: One component product-no mixing requiredFast cure at elevated temperaturePrimerless adhesion to many types of substratesNo cure by-products, low linear shrinkageNon-corrosive to metals and sensitive substratesExcellent dielectric propertiesOutstanding performance over a wide thermal range GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Viscosity 55000 cP
55000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 28
28
Tensile Strength, Ultimate 2.35 MPa
341 psi
Elongation at Break 290 %
290 %
Adhesive Bond Strength 1.96 MPa
284 psi
Aluminum to aluminum
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
Dielectric Constant 2.8
2.8
Dielectric Strength 21.02 kV/mm
533.9 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
90.0 min

@Temperature 125 °C
1.50 hour

@Temperature 257 °F
180 min

@Temperature 100 °C
3.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Color Translucent
Consistency Flowable