Polymer Property : Adhesive Bond Strength = 284 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.96 MPa
284 psi
Aluminum to aluminum
Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive
TSE 3221 is a one-component, flowable, heat curing adhesive which is translucent in color and offers primerless adhesion to a wide variety of substrates. This product requires an elevated temperatur..
Adhesive Bond Strength 1.96 MPa
284 psi
Aluminum to aluminum
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit..
Adhesive Bond Strength 1.96 - 2.94 MPa
284 - 426 psi
Transverse
Pyrotek Pyromoldable JDR1150A Moldable Paste Type Low Density Refractory
ApplicationsLaunder linings Lining of distribution launders for DC casting table Industrial furnace linings Back up material behind hot face lining AdvantagesLow density with high insulating propert..