Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Mid-Mountain Materials
Trade Name PADMAT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation materials that are available in a wide range of thicknesses. MT1000 is light weight, strong, and highly efficient as insulation in most high heat environments for extended periods at elevated. The absence of organic or synthetic binders makes this product smoke free on heat up and allows the product to remain mechanically stable even after exposure to extreme temperatures.Characteristics: Non combustibleGood drapabilityWill not contribute to metal corrosionWill not decay, not sustain mold or verminExcellent vibration resistanceOdorless - will not absorb odorsExcellent sound absorption qualitiesFlame spread / smoke generated - 0/0Information provided by Mid-Mountain Materials.
Physical Properties Metric English Comments
Density 0.0961 - 0.192 g/cc
0.00347 - 0.00694 lb/in³
Thickness 3180 - 25400 microns
125 - 1000 mil
nom
Thermal Properties Metric English Comments
Thermal Conductivity 0.0576 W/m-K

@Temperature 149 °C
0.400 BTU-in/hr-ft²-°F

@Temperature 300 °F
0.0720 W/m-K

@Temperature 260 °C
0.500 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.0937 W/m-K

@Temperature 371 °C
0.650 BTU-in/hr-ft²-°F

@Temperature 700 °F
Melting Point 1120 °C
2050 °F
Maximum Service Temperature, Air 538 °C
1000 °F
Continuous
816 °C
1500 °F
Short Term
Descriptive Properties Value Comments
Construction Needled & Felted Blanket
Material High purity E-Glass
Width 60 inches