Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech APET SP4110 Copolyester Sheet

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Spartech
Trade Name APET
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech APET SP4110 Copolyester Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyester SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 106
106
ASTM D2240
Tensile Strength at Break 57.9 MPa
8400 psi
ASTM D882
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D882
Elongation at Break 300 %
300 %
ASTM D882
Tensile Modulus 2.21 GPa
320 ksi
ASTM D882
Flexural Yield Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Unnotched 0.497 J/cm
0.930 ft-lb/in
ASTM D256
0.278 J/cm

@Temperature -40.0 °C
0.520 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 678 J
500 ft-lb
73°F; ASTM D1709A
542 J

@Temperature -40.0 °C
400 ft-lb

@Temperature -40.0 °F
ASTM D1709A
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM E540
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523
Users viewing this material also viewed the following: