Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3180 microns | 125 mil | Standard |
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:.. |
|||
Thickness | 3180 microns | 125 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF90 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 3180 - 25400 microns | 125 - 1000 mil | nom |
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation material.. |
|||
Thickness | 3180 microns | 125 mil | ASTM D374, method D, using 17 N/cm² |
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |
|||
Thickness | 3180 microns | 125 mil | injection molded |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4318 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4508 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber Product Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silic.. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Natural (Transparent)Interleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Inform.. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10842R125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by .. |
|||
Thickness | 3180 microns | 125 mil | Overall Thickness |
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma.. |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | Composite-Pad; ASTM D1000 |
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | 3180 microns | 125 mil | Composite-Pad; ASTM D1000 |
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4108 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4108 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | ASTM D1000 |
3M Scotchfil™ Electrical Insulation Putty 3M™ Scotchfil™ Electrical Insulation Putty is used as a build-up compound on highly irregular surfaces such as fittings and valves, providing a smooth, waterproof taping surface. The putty is soft.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4718 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 - 12700 microns | 125 - 500 mil | Range of Thicknesses Available |
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applicatio.. |
|||
Thickness | 3180 microns | 125 mil | Rubber |
Arlon 30850N125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |