Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 25400 microns | 0.500 - 1000 mil | Average value: 316 microns Grade Count:504 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thickness | 3180 - 25400 microns | 125 - 1000 mil | nom |
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation material.. |