Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material
Manufacturer Microtherm Group
Trade Name Marineguard®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are the basis of the ultra lightweight Microtherm® passive fire protection systems for all modes of transportation.PropertiesOpacified blend of filament reinforced silicaLightweight flexible overstitched panels of microporous insulationCertified to internationally recognized standards including IMO and USCGCertified non combustibleCertified Class A1 to European Single Burning Item (SBI) test, EN 13823Stable performance for fire exposureClean and environmentally safeTypical ApplicationsMarine PFP to bulkheads and decks - standard aluminum, lightweight aluminum, steel, compositesFire protection to piping systems - fast fittingPassive fire protection to rail applications - lightest systems for aluminium carriage floorsInformation provided by Microtherm.
Physical Properties Metric English Comments
Density 0.200 - 0.300 g/cc
0.00723 - 0.0108 lb/in³
Thickness 4000 - 10000 microns
157 - 394 mil
Thermal Properties Metric English Comments
Specific Heat Capacity 0.680 J/g-°C

@Temperature 0.000 °C
0.163 BTU/lb-°F

@Temperature 32.0 °F
0.920 J/g-°C

@Temperature 200 °C
0.220 BTU/lb-°F

@Temperature 392 °F
1.00 J/g-°C

@Temperature 400 °C
0.239 BTU/lb-°F

@Temperature 752 °F
Thermal Conductivity 0.0258 W/m-K

@Temperature 100 °C
0.179 BTU-in/hr-ft²-°F

@Temperature 212 °F
@ 240 kg/m³, cell pitch of 50mm
0.0283 W/m-K

@Temperature 200 °C
0.196 BTU-in/hr-ft²-°F

@Temperature 392 °F
@ 240 kg/m³, cell pitch of 50mm
0.0313 W/m-K

@Temperature 300 °C
0.217 BTU-in/hr-ft²-°F

@Temperature 572 °F
@ 240 kg/m³, cell pitch of 50mm
0.0347 W/m-K

@Temperature 400 °C
0.241 BTU-in/hr-ft²-°F

@Temperature 752 °F
@ 240 kg/m³, cell pitch of 50mm
Maximum Service Temperature, Air 1000 °C
1830 °F
for long term exposure