Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0500 - 0.300 g/cc | 0.00181 - 0.0108 lb/in³ | Available range |
MarkeTech Silica Aerogel Silica aerogels are generally known for being an extremely lightweight transparent solid down to |
|||
Density | 0.200 - 0.300 g/cc | 0.00723 - 0.0108 lb/in³ | |
Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are .. |
|||
Density | 0.260 - 0.300 g/cc | 0.00939 - 0.0108 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 445 CDN CR-Neoprene Foam Polychloroprene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.250 - 0.300 g/cc | 0.00903 - 0.0108 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D1 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |