Dow Corning 1503 Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 1503 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A blend of an ultra high viscosity dimethiconol in a low viscosity dimethicone fluid for use in skincare, woundcare, scar therapy, suncare, and color cosmetic applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc

@Temperature 25.0 °C
0.920 g/cc

@Temperature 77.0 °F
Viscosity Measure 1500 cSt
1500 cSt
kinetic/kinematic
Thermal Properties Metric English Comments
Flash Point >= 105 °C
>= 221 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.397
1.397
Processing Properties Metric English Comments
Shelf Life 30.0 Month
30.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Cyclotetrasiloxane Content (max %) 0.94