Physical Properties Metric English Comments
Thickness 4000 - 10000 microns
157 - 394 mil
Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof
Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are ..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 4000 - 4500 microns
157 - 177 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..