Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Dry Air |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Dry Air |
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | for Continuous use with specialty cloth exterior or flexible core |
Pyrotek MT-29Q Quilted Microporous Insulation MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains .. |
|||
Maximum Service Temperature, Air | 1000 °C @Pressure 6.89 MPa |
1832 °F @Pressure 1000 psi |
Continuous |
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | resists oxidation |
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1832 °F | |
Stellar Canada CERAMITE® CSR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Recommended Operating Temperature |
Unifrax Excelfrax® 1800 Board Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Safe Operating Temp |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Chosun Refractories AH-5 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | limited |
Chosun Refractories MIX-3 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | no load |
Astro Met Macor® Machinable Glass Ceramic General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Continuous |
Pyrotek MT-29B Microporous Insulating Board MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |