Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 10000 microns | 0.500 - 394 mil | Average value: 1440 microns Grade Count:15 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Thickness | 4000 - 10000 microns | 157 - 394 mil | |
Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are .. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8000 - 10000 microns | 315 - 394 mil | |
Beijing Evergrow Resources BF-10 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 9500 - 10000 microns | 374 - 394 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |