Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron

Category Metal , Ferrous Metal , Cast Iron , Alloy Cast Iron , Ductile Iron
Manufacturer Meehanite
Trade Name Ductliron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is readily machinable and responds easily to surface hardening by chill casting or by flame or electric induction heat treatment.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Physical Properties Metric English Comments
Specific Gravity 7.20 g/cc
7.20 g/cc
Mechanical Properties Metric English Comments
Hardness, Brinell 200
200
Nominal
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Tensile Strength, Yield 414 - 517 MPa
60000 - 75000 psi
Elongation at Break 3.0 - 10 %
3.0 - 10 %
Modulus of Elasticity 172 GPa
25000 ksi
Poissons Ratio 0.37
0.37
Fatigue Strength 269 MPa
39000 psi
Endurance Limit (Unnotched)
Shear Modulus 62.8 GPa
9110 ksi
Calculated
Thermal Properties Metric English Comments
Shrinkage 1.3 %
1.3 %
Patternmaker Shrinkage