Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 580 - 690 MPa | 84100 - 100000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30T 74-79Tabulated properties appl.. |
|||
Tensile Strength, Ultimate | 621 - 689 MPa | 90000 - 100000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 414 - 689 MPa | 60000 - 100000 psi | |
Meehanite CHS Corrosion Resisting Cast Iron Type CHS is a higher strength material with good shock resistance. Compositional adjustments are made to suit exact service requirements. Recommended for use for components subjected to concentrat.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 627 - 689 MPa | 91000 - 100000 psi | |
Eagle Brass 260 Cartridge Brass, Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Eagle Brass 70265 XP175, Annealed Information provided by Eagle Brass Company |