Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Pacific Sintered Materials F-240-S(HT) Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-60(HT)All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
PSM Industries Pacific Sintered Metals Steel F-240-S(HT) Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-60(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Ultimate | 552 - 1240 MPa | 80000 - 180000 psi | |
Meehanite Ductliron® AQS Nodular Graphite Ductile Iron Type AQS is an air hardening metal possessing high strength, toughness and hardness. It may be fully air quenched throughout casting section after machining to a wide range of strength and hardness.. |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 182 Nickel Alloy Welding Wire Alloy 182 is used for arc welding Inconel types 600 and 601 to themselves or one to another. Deposited weld metal meets the most stringent radiographic requirements. Alloy 182 dissimilar welding app.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 320 Stainless Steel Electrode Universal 320 produces a fully austenitic deposit for welding Carpenter Stainless No. 20Cb-3 (wrought form) or Durimet 20 (cast form) or similar alloys. The 320 alloy was developed to give improved .. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 80SB-2 Steel Welding Wire Universal 80SB-2 is a 1/14 chromium 2 molybdenum alloy designed for welding similar composition alloys used primarily in the process industries in steam piping systems and pressure vessels. Weld dep.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 80SB-2L Steel Welding Wire Universal 80SB-2L is the same as 80SB-2 with the exception of the carbon content, which is restricted to less than 0.05%.Universal 80SB-2 is a 1/14 chromium 2 molybdenum alloy designed for welding s.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 82 Nickel Alloy Welding Wire Alloy 82 is used for TIG, MIG and submerged-arc welding of Inconel type alloys 600 and 601, Incoloy type alloy 800 and welding the clad side of steel clad with nickel chromium alloy. Dissimilar meta.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works A Nickel Alloy Welding Wire Alloy A is used for arc welding various dissimilar combinations of austenitic and ferritic steels and high nickel alloys. For example, when welding Inconel and Incoloy type alloys to carbon steel, s.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Me.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | As Welded |
Universal Wire Works Inconel 92 (AMS 5675) Nickel Alloy Filler Metal Inconel Filler Metal 92 is a nickel base alloy designed especially for gas tungsten arc and gas metal arc welding of dissimilar combinations of high nickel alloys and austenitic and ferritic steels... |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 70S-2 Steel Welding Wire Universal 70S-2 is designed for TIG or MIG welding of all carbon steels. The tensile strength exceeds the base metal on single pass deposits on gaged carbon steel. Alloy 70S-2 is triple deoxidized u.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Tritex TREO Needled Blanket Insulation Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries.. |
|||
Tensile Strength, Ultimate | 552 - 565 MPa | 80000 - 82000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Eagle Brass 7026 Copper Nickel, Annealed 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Eagle Brass 70265 XP175, Annealed Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 552 - 634 MPa | 80000 - 92000 psi | |
Eagle Brass 715 Copper Nickel 30%, Extra Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Ultimate | 552 - 655 MPa | 80000 - 95000 psi | |
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Crucible Steel 304L Chromium-Nickel Steel Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | cold worked |
CMW® ELKONIUM 1 silver, copper, nickel alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | cold worked |
CMW® ELKONIUM 22 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Tensile Strength, Ultimate | 552 MPa | 80000 psi | |
Universal Wire Works 132 Nickel Alloy Welding Wire Alloy 132 is used for arc welding Inconel type alloy 600 and 601 and stainless alloy 330. Deposited weld metal has excellent high temperature strength and oxidation resistance. The dissimilar weldin.. |