Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 62.8 GPa | 9110 ksi | Calculated |
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r.. |