Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 621 - 689 MPa | 90000 - 100000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 414 - 689 MPa | 60000 - 100000 psi | |
Meehanite CHS Corrosion Resisting Cast Iron Type CHS is a higher strength material with good shock resistance. Compositional adjustments are made to suit exact service requirements. Recommended for use for components subjected to concentrat.. |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r.. |
|||
Tensile Strength, Ultimate | 414 - 689 MPa | 60000 - 100000 psi | |
Meehanite HS Heat Resisting Cast Iron Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 627 - 689 MPa | 91000 - 100000 psi | |
Eagle Brass 260 Cartridge Brass, Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Eagle Brass 7026 Copper Nickel, Annealed 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 552 - 689 MPa | 80000 - 100000 psi | |
Eagle Brass 70265 XP175, Annealed Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |