Shear Modulus 62.8 GPa
9110 ksi
Calculated
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r..