Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Niagara LaSalle 1212 Cold Finished Steel Bar This is basic screw machine steel. The grade is used as a standard of comparison for machinability (1212 is rated as 100%). It machines easily, provides good surface finish and has good brazing prop.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Niagara LaSalle 1213 Cold Finished Steel Bar The A.I.S.I. grade 1215 has essentially eliminated a number of similar free machining grades, such as 1212. Both 1215 and 1213 machine considerably faster than 1212 and provide good surface finish a.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Pacific Sintered Materials FCC-214-S High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 414 MPa @Temperature 23.9 °C |
60000 psi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Yield | 414 - 483 MPa @Strain 0.200 % |
60000 - 70000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 414 - 517 MPa | 60000 - 75000 psi | |
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 %, Temperature 260 °C |
60000 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
Heat Treated |
Universal Wire Works 29-9 (AMS 5784) Filler Metal Universal 29-9 is designed for welding similar and dissimilar corrosion and heat resisting steels with the gas metal arc and gas tungsten arc welding processes.Information provided by Universal Wire.. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | |
ThyssenKrupp 12Ni5 Structural Steel 5% nickel steel for low temperature service down to -165°FApplication for pressure vessels and tanks for the transportation and storage of ethyleneReference: 5.000 t/y in thicknesses up to 2 in.Hea.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | AR-5% O2 |
Universal Wire Works ER90SB-9 Steel Welding Wire Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The adv.. |
|||
Tensile Strength, Yield | >= 414 MPa @Strain 0.200 % |
>= 60000 psi @Strain 0.200 % |
|
Universal Wire Works Inconel 625 (AMS 5837) Filler Metal Inconel Filler Metal 625 is recommended for gas metal arc and gas tungsten arc welding of nickel base alloys 625 and 601, Incoloy alloys, carbon steels, low alloy steels and stainless steels. This a.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal Inconel Filler Metal 718 is recommended for gas tungsten arc and gas metal arc welding of alloy 718, 706 and X-750. This double gamma prime alloy has excellent strength, good ductility up to 1300°F.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should .. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | 0.2% offset |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Yield | 414 - 462 MPa | 60000 - 67000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 414 - 538 MPa | 60000 - 78000 psi | 0.2% Offset |
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Tensile Strength, Yield | 414 - 538 MPa | 60000 - 78000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick) |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr Low carbon, nickel containing, dual phase 12% Cr stainless steel alloy. Characteristics: superior toughness to ferritic alloys, high strength, high corrosion resistance.Information provided by Alleg.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal Data provided by Allvac.Applications: High temperature applications, jet engine components, devices in high fatigue service. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | For flat products (<4" thickness) and seamless tube and pipe |
ATI Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625 Allegheny Ludlum Altemp 625 alloy is an austenitic nickel-base superalloy possessing excellent resistance to oxidation and corrosion over a broad range of corrosive conditions, including jet engine .. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 %, Temperature 260 °C |
60000 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |