Master Bond EP76M Nickel Filled Electrically Conductive Epoxy System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP76M Nickel Filled Electrically Conductive Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP76M is a two component, nickel filled, electrically conductive adhesive for high performance bonding, sealing, and coating formulated to cure at room temperature or more rapidly at elevated temperatures. Unlike the majority of two part nickel conductive systems, EP76M has a one-to-one mix ratio by weight or volume.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.0 °C
24.0 - 48.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Gray; "B" Gray
Mix Ratio By Weight 100/100
Set-Up Time, minutes 60
At Room Temperature
Viscosity Paste
Room Temperature