Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 120 - 180 min @Temperature 65.0 °C |
2.00 - 3.00 hour @Temperature 149 °F |
|
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Cure Time | 60.0 - 180 min @Temperature 23.0 °C |
1.00 - 3.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Cure Time | 60.0 - 180 min @Temperature 23.0 °C |
1.00 - 3.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Cure Time | 60.0 - 180 min @Temperature 23.0 °C |
1.00 - 3.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Cure Time | 60.0 - 180 min @Temperature 23.0 °C |
1.00 - 3.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Cure Time | 120 - 180 min @Temperature 25.0 °C |
2.00 - 3.00 hour @Temperature 77.0 °F |
Tack Free; 50% relative humidity |
Lord Adhesives Aeroglaze® Z306 Absorptive Polyurethane Aeroglaze® Z306 absorptive polyurethane coating is primarily for applications to substrates used in space operations. These operations include those where coatings must exhibit low outgassing cha.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21TDC-2ND Two component, highly flexibilized, non-drip epoxy resin compound Product Description: Master Bond EP21TDC-2ND is a two component highly flexible epoxy resin system for high performance bonding, sealing and coating with a non-drip consistency. It has a forgiving o.. |
|||
Cure Time | 120 - 180 min @Temperature 65.6 °C |
2.00 - 3.00 hour @Temperature 150 °F |
|
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP30DPMed USP Class VI, Two Component Epoxy Urethane System Master Bond Polymer System EP30DPMED is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding,.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Cure Time | 120 - 180 min @Temperature 121 - 149 °C |
2.00 - 3.00 hour @Temperature 250 - 300 °F |
|
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21BAS Radiopaque Two Component Epoxy Master Bond Polymer System EP21BAS is a radiopaque epoxy compound which offers outstanding performance and superior processability. Radiopaque epoxy polymer compounds are employed for medical diagno.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21CLV Two Component Epoxy System Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu.. |
|||
Cure Time | 120 - 180 min @Temperature 93.3 °C |
2.00 - 3.00 hour @Temperature 200 °F |
|
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive Description: Master Bond Polymer System Supreme 33 is a unique, room temperature curing, toughened epoxy adhesive/sealant, offering high temperature resistance. This innovative system offers high bo.. |
|||
Cure Time | 120 - 180 min @Temperature 100 °C |
2.00 - 3.00 hour @Temperature 212 °F |
|
Abatron AboCast 8103-21 High-Performance Dielectric Epoxy AboCast 8103-21 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines r.. |
|||
Cure Time | 30.0 - 180 min @Temperature 50.0 - 100 °C |
0.500 - 3.00 hour @Temperature 122 - 212 °F |
Optional |
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound AboCoat 8401-1 A/B is a conventional highly-filled coating to produce conductive paths with the highest silver content possible. It requires strict controls. Resistivity may rise to 0.1 ohm/sq under.. |
|||
Cure Time | 30.0 - 180 min @Temperature 50.0 - 100 °C |
0.500 - 3.00 hour @Temperature 122 - 212 °F |
|
Abatron AboCoat 8709-8/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound AboCoat 8709-8/AboCure 50-12 is a versatile nickel-epoxy conductive coating. |
|||
Cure Time | 120 - 180 min @Temperature 100 °C |
2.00 - 3.00 hour @Temperature 212 °F |
|
Abatron AboCast 8103-20 High-Performance Dielectric Epoxy AboCast 8103-20 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is unique .. |
|||
Cure Time | 120 - 180 min @Temperature 100 °C |
2.00 - 3.00 hour @Temperature 212 °F |
|
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Cure Time | 60.0 - 180 min @Temperature 23.0 °C |
1.00 - 3.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond MH052 Anaerobic Threadsealant Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1.. |